The method of forming the cured fine particles includes preparing an uncured poly(glycerol sebacate) resin. The method also includes forming the composition into a plurality of uncured microparticles and curing the uncured microparticles to form a plurality of cured microparticles. The uncured microparticles do not contain a photoinduced crosslinking agent. The method of forming the scaffolding material includes providing microparticles that include a three-dimensional array of poly(glycerol sebacate). The method also includes stimulating the three-dimensional array of particles to sinter the particles, thereby forming a scaffolding material having a plurality of pores. The scaffolding material is formed from a plurality of microparticles containing a three-dimensional arrangement of poly(glycerol sebacate) thermosetting resin. The scaffold material has a plurality of pores. [Selection diagram] Figure 4硬化微粒子を形成する方法は、未硬化状態のポリ(グリセロールセバケート)樹脂を用意することを含む。この方法はまた、組成物を複数の未硬化微粒子に形成すること、及び未硬化微粒子を硬化させて複数の硬化微粒子を形成することを含む。未硬化の微粒子は、光誘起架橋剤を含まない。足場材料を形成する方法は、3次元配置のポリ(グリセロールセバケート)を含む微粒子を用意することを含む。この方法はまた、3次元配置の微粒子を刺激して微粒子を焼結させ、それによって複数の細孔を有する足場材料を形成することを含む。足場材料は、3次元配置のポリ(グリセロールセバケート)熱硬化性樹脂を含む複数の微粒子から形成される。足場材料は複数の細孔を有する。【選択図】図4