PROBLEM TO BE SOLVED: To provide a coating-treated powder obtained by coating-treating a powder with a raw material derived from vegetable oil-and-fat that has no concern about generation of offensive odor with the lapse of time, can be incorporated with a cosmetic, has a very smooth touch feeling and is excellent in water repellency and pigment dispersibility, and to provide a cosmetic comprising the coating-treated powder.SOLUTION: The coating-treated powder is obtained by coating-treating a powder to be treated with a mixture, as a coating-treating agent, comprising 60-90 wt.% of an extremely hardened vegetable oil-and-fat having a melting point of 50°C or higher and 10-40 wt.% of an ester oil agent derived from vegetable oil-and-fat. Preferably, the powder is coating-treated at a temperature 10-20°C higher than the melting point of the extremely hardened vegetable oil-and-fat when coating-treated with the coating-treating agent. The powder to be treated is coating-treated with the coating-treating agent in an amount of preferably 1-15 wt.%, particularly preferably 3-10 wt.%. The cosmetic is obtained by using the coating-treated powder as a part or the whole of components thereof.COPYRIGHT: (C)2011,JPO&INPIT【課題】植物油脂由来の原料を使って粉体へ被覆処理をする際に経時的な異臭発生の問題が無く、化粧料に配合することができ、非常に滑らかな感触を持ち、撥水性、顔料分散性に優れた被覆処理粉体の提供、及び、その被覆処理粉体を配合した化粧料を提供する。【解決手段】被処理粉体へ、融点が50℃以上の植物性極度硬化油脂60重量%~90重量%と植物油脂由来のエステル油剤10重量%~40重量%とからなる混合物を被覆処理剤として被覆処理することによって得られる被覆処理粉体。被覆処理剤を被覆処理する際に、植物性極度硬化油脂の融点より10~20℃高い温度にて被覆処理することが好ましい。被処理粉体を被覆処理剤1重量%~15重量%、特に好ましくは3重量%~10重量%の量で被覆処理することが好ましい。さらに本被覆処理粉体を化粧料の成分の一部、もしくは全部として用い化粧料を得ることができる。【選択図】なし