The present invention relates to a process for preparing a chitosan-based neutralized compressed porous layer comprising the following steps: a) preparing a solution of chitosan; b) pouring said solution into a mold in order to form a layer; c) the layer obtained in b) is lyophilized to obtain a porous layer; d) the said porous layer obtained in c) is compressed; and e) the compressed porous layer obtained in d) is neutralized by means of a solution. of NH OH. It also relates to an implant comprising a layer obtained by such a method.La présente invention porte sur un procédé de préparation d'une couche poreuse compressée neutralisée à base de chitosane comprenant les étapes suivantes : - a) on prépare une solution de chitosane, - b) on verse dans un moule ladite solution afin de former une couche, - c) on lyophilise la couche obtenue en b) pour obtenir une couche poreuse, - d) on compresse ladite couche poreuse obtenue en c), - e) on neutralise la couche poreuse compressée obtenue en d) au moyen d'une solution de NH OH. Elle porte également sur un implant comprenant une couche obtenue selon un tel procédé.