How To create the coatable composition, a) comprising the steps of: providing an initial composition containing dispersed silica particles in an aqueous liquid medium, the average particle diameter of silica particles is less than 100 nanometers having a particle size distribution having a silica sol having a greater than 6 pH, step, b) and 4 acidified to a pH below the initial composition with inorganic acids, providing a acidified composition , and c) by dissolving at least one metal compound in a composition which is the acidification, the step of providing a coating composition, a. At least one metal compound comprises a silver compound, a zinc compound, and at least one copper compound. The coating composition can be prepared by this method, the antimicrobial compositions are also disclosed. Antimicrobial article comprising the antimicrobial composition are also disclosed.FIELD 1コーティング可能な組成物を作成する方法は、a)水性液媒中に分散されたシリカナノ粒子を含む初期組成物を提供する工程であって、シリカナノ粒子は100ナノメートル以下の平均粒子径を有する粒子径分布を有し、シリカゾルは6より大きいpHを有する、工程、b)無機酸を用いて初期組成物を4以下のpHまで酸性化して、酸性化された組成物を提供する工程、及びc)その酸性化された組成物中に少なくとも1種の金属化合物を溶解して、コーティング可能な組成物を提供する工程、を含む。少なくとも1種の金属化合物は、銀化合物、亜鉛化合物、及び銅化合物の少なくとも1つを含む。この方法により調製可能なコーティング可能な組成物、抗菌性組成物もまた開示される。抗菌性組成物を含む抗菌性物品もまた開示される。【選択図】 図1