PROBLEM TO BE SOLVED: To provide: a stent manufacturing method capable of obtaining a stent having excellent sludge resistance, by forming a smooth coating layer having low irregularity by improving wettability of a coating surface on which coating with coating liquid is to be performed and a stent obtained by using the manufacturing method.SOLUTION: A manufacturing method for a stent comprising a stent body composed of a cylindrical metal mesh tube and a cover member covering the outer periphery and/or inner periphery of the stent body or a stent constituted by a cylindrical resin tube includes: a plasma irradiation step of irradiating the inner periphery of the cover member or an inner periphery 31S of the resin tube with plasma J and a coating step of performing coating with coating liquid containing a polymer obtained by polymerizing 2-methoxyethyl acrylate or methoxy acrylate-based derivative on the inner periphery of the cover member or the inner periphery 31S of the resin tube after the plasma irradiation.SELECTED DRAWING: Figure 1COPYRIGHT: (C)2017,JPO&INPIT【課題】コーティング液をコーティングするコーティング面の濡れ性を改善して、凹凸の少ない滑らかなコーティング層を形成し、耐スラッジ性に優れたステントを得ることができる、ステントの製造方法、及び該製造方法によって得られるステントを提供する。【解決手段】筒状の金属メッシュチューブからなるステント本体と、ステント本体の外周及び/又は内周を覆うカバー部材とを備えたステント、又は、筒状の樹脂チューブで構成されたステントの製造方法であって、カバー部材の内周又は樹脂チューブの内周31SにプラズマJを照射するプラズマ照射工程と、プラズマ照射後の前記カバー部材の内周又は樹脂チューブの内周31Sに、アクリル酸2-メトキシエチル又はアクリル酸メトキシ系誘導体を重合して得られるポリマーを含むコーティング液をコーティングするコーティング工程とを含む。【選択図】図1