摘要:
PROBLEM TO BE SOLVED: To provide a spherical silica having a high oil absorption amount, a suitable specific surface area and a spherical particle shape.SOLUTION: The spherical silica has an oil absorption amount of 580 ml/100 g or more and a specific surface area of 200-400 m2/g. The spherical silica preferably has 10-100 μm of a particle size having the total volume of 50% when the volume of particles is integrated from the side of a small particle size and more preferably has 1.7 or less of a ratio of (a particle size having the total volume of 90% when the volume of the particles is integrated from the side of a small particle size)/(a particle size having the total volume of 10% when the volume of the particles is integrated from the side of a small particle size).COPYRIGHT: (C)2015,JPO&INPIT【課題】吸油量が高く、適当な比表面積で、粒子形状が球状である、球状シリカを提供することである。【解決手段】吸油量が580ml/100g以上であり、比表面積が200~400m2/gである、球状シリカである。より好ましくは、この球状シリカは、粒子の体積を粒子径の小さな側から積算していった場合に合計体積の50%となるときの粒子径が10~100μmである。より好ましくは、この球状シリカは、(粒子の体積を粒子径の小さな側から積算していった場合に合計体積の90%となるときの粒子径)/(粒子の体積を粒子径の小さな側から積算していった場合に合計体積の10%となるときの粒子径)が1.7以下である。【選択図】図1
来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充