摘要:
The present invention provides a calcium cement-based bone substitute material which is safer than conventional bone substitute materials and is capable of promoting regeneration of bone tissues by means of infiltration of osteoblasts.The present invention specifically provides a paste for forming a bone substitute porous body, which contains tricalcium α-phosphate, castor oil and water. The paste for forming a bone substitute porous body is characterized in that the tricalcium α-phosphate has a particle diameter of 10-50 μm and the tricalcium α-phosphate is contained in an amount of 30-50% by weight.La présente invention concerne un matériau de substitut osseux à base de ciment de calcium, qui est plus sûr que les matériaux de substitut osseux classique et est apte à favoriser la régénération de tissus osseux par linfiltration dostéoblastes. La présente invention concerne plus spécifiquement une pâte destinée à former un corps poreux de substitut osseux, contenant du phosphate α tricalcique, de lhuile de ricin et de leau. Ladite pâte destinée à former un corps poreux de substitut osseux se caractérise en ce que le phosphate α tricalcique présente un diamètre de particule compris entre 10 et 50 μm, et en ce que le phosphate α tricalcique est contenu dans une quantité comprise entre 30 et 50 % en poids.本発明は、カルシウムセメント系の骨置換材料であって、従来品よりも安全性が高く且つ骨芽細胞の浸潤による骨組織の再生を促進できる骨置換材料を提供する。 本発明は、具体的には、α-リン酸三カルシウム、ヒマシ油及び水を含有する骨置換多孔質体形成用ペーストであって、前記α-リン酸三カルシウムの粒子径が10~50μmであり、前記α-リン酸三カルシウムの含有量が30~50重量%であることを特徴とするペーストを提供する。
来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充