The present invention provides the following: a covered flux which has a low chromium content and which can improve the fatigue strength of a weld in additional welding; and a covered electrode. The covered flux used for a covered electrode has a composition that contains, relative to the total mass of the covered flux, 35-55 mass % of a metal carbonate (in terms of CO 2 ), 10-30 mass % of a metal fluoride (in terms of F), and 8.5-20 mass % of Mn and/or 7.5-20 mass % of Ni. In addition, the covered electrode is obtained by coating an iron-based core wire with this covered flux.