DBM compositions, methods of manufacture, and methods of treatment using the same. The DBM composition is made from a mechanically entangled bone material that does not contain a carrier. Agglomerates of mechanically entangled desalted bone fibers can be obtained by needle punching into a barbed needle, entanglement with water or air jets, or by applying ultrasonic waves to desalted bone fibers. Agglomerates of mechanically entangled desalted bone fibers can also be obtained by application of the moisture, heat and pressure provided by the pressure rollers to the desalted bone fibers. A method of making a bone material for hydration into a liquid is provided. The method comprises applying mechanical entanglement to the desalted bone fibers to obtain aggregates of carrier-free demineralized bone fibers.DBM 조성물, 제조 방법, 및 이를 사용한 치료 방법이 제공된다. DBM 조성물은 캐리어를 함유하지 않는 기계적으로 얽힌 뼈 재료로부터 제조된다. 기계적으로 얽힌 탈염된 뼈 섬유의 응집체는 미늘 니들로의 니들 펀칭, 물 또는 공기 제트로의 얽힘에 의해, 또는 초음파를 탈염된 뼈 섬유에 적용함으로써 수득될 수 있다. 기계적으로 얽힌 탈염된 뼈 섬유의 응집체는 또한 압력 롤러에 의해 제공되는 수분, 열 및 압력의 탈염된 뼈 섬유에의 적용에 의해 수득될 수 있다. 액체로 수화하기 위한 뼈 재료의 제조 방법이 제공된다. 상기 방법은 탈염된 뼈 섬유에 기계적 얽힘을 가하여 캐리어가 없는 탈염된 뼈 섬유의 응집체를 수득하는 단계를 포함한다.