I to provide a composition that gives the molded article [challenge] heat resistance, liquid-leakage resistance and needle retention is excellent. Block copolymer weight having a block derived from styrene controlled distribution copolymer - butadiene from 50 to 95 parts by weight, and styrene polymer block the block copolymer A having a butadiene-derived polymer block and [MEANS FOR SOLVING PROBLEMS] styrene polymer block 100 to 300 parts by weight of a softening agent B is 50~500cSt 5~50 parts by weight (total weight of the block copolymer and P block copolymer A is 100 parts by weight), a kinematic viscosity at 40 ℃ coalescence P, and to provide a medical container plug body for elastomer composition of 1 to 50 parts by mass of propylene polymer C is 1000~3000MPa flexural modulus. None [Selection Figure]【課題】耐熱性、耐液漏れ性および針保持性が優れる成形体を与える組成物を提供する。【解決手段】スチレン重合体ブロックおよびブタジエン由来重合体ブロックを有するブロック共重合体Aを50~95質量部、スチレン重合体ブロックおよびブタジエン-スチレン制御分布共重合体に由来するブロックを有するブロック共重合体Pを5~50質量部(ブロック共重合体Aおよびブロック共重合体Pの合計量は100質量部)、40℃における動粘度が50~500cStである軟化剤Bを100~300質量部、および曲げ弾性率が1000~3000MPaであるプロピレン重合体Cを1~50質量部含有する医療容器栓体用エラストマー組成物を提供する。【選択図】 なし