遺伝子とリン酸カルシウムを含む複合粒子を備える遺伝子導入用基材
专利权人:
NATIONAL INSTITUTE OF ADVANCED INDUSTRIAL & TECHNOLOGY
发明人:
OYANE AYAKO,大矢根 綾子,ARAKI HIROKO,荒木 裕子,ITO ATSUO,伊藤 敦夫,SOGO TOMO,十河 友,TSURUSHIMA HIDEO,鶴嶋 英夫,SUBHADIP BODHAK,シュバディップ ボダック
申请号:
JP2012199854
公开号:
JP2014054326A
申请日:
2012.09.11
申请国别(地区):
JP
年份:
2014
代理人:
摘要:
PROBLEM TO BE SOLVED: To provide a gene introduction base material that can introduce a gene in a cell on a base material with high efficiency.SOLUTION: A production method of a gene introduction base material includes a process in which a base material is made to contact a supersaturated calcium phosphate solution including a gene at 20-40°C, a composite particle including the gene and calcium phosphate formed in the solution is subjected to precipitation and immobilization on a surface of the base material, and a layer comprising the composite particle is formed on the base material surface, wherein a supersaturated calcium phosphate solution including the gene includes: 1-100 μg/mL of a gene 1.8-5.5 mM of a Ca component 0.9-2.8 mM of a P component 10-200 mM of a K and/or Na component (summation) and 10-200 mM of a Cl component as an initial concentration.COPYRIGHT: (C)2014,JPO&INPIT【課題】本発明は、基材上の細胞に高効率的に遺伝子導入することが可能な遺伝子導入用基材を提供することを目的とする。【解決手段】本発明は、遺伝子導入用基材の製造方法であって、基材を、遺伝子を含むリン酸カルシウム過飽和溶液と、20~40℃にて接触させ、該溶液中で形成された、該遺伝子とリン酸カルシウムを含む複合粒子を該基材表面に沈降及び固定化し、該基材表面に該複合粒子からなる層を形成する工程を含み、該遺伝子を含むリン酸カルシウム過飽和溶液が、初期濃度として、遺伝子1~100μg/mL、Ca成分1.8~5.5mM、P成分0.9~2.8mM、K及び/又はNa成分(合算)10~200mM、、並びに、Cl成分10~200mMを含む、上記方法に関する。【選択図】なし
来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充