Smoke is reduced during manufacture of the nonwoven fabrics, moreover, moreover object of the present invention is to develop a non-woven fibers and suitable for olefin polymer nonwoven fabric durability and hydrophilic initial hydrophilicity better together. The present invention, and poly 0.5-5 parts by weight (oxyalkylene) sorbitan fatty acid ester di for poly olefin polymer 100 parts by weight, represented by the following chemical formula (1) (oxyalkylene) diol (alkylene group is a butylene or propylene or ethylene, addition mole number from 10 to 40, the fatty acid. alkylene is a fatty acid alkyl, or 12 to 18 carbon atoms) fatty acid ester 0.01 to 2.5 birds a It is intended to provide a fiber made from an olefin polymer composition comprising a weight. R 1 -COO- (C n H 2n O) a -C 6 H 12 -O (C n H 2n O) b -CO-R 2 · · · · Formula (1) Wherein the number of carbon atoms is an alkyl group, of 11 to 17 R 2 and R 1, even in the same respectively, to be different well, and (C n H 2n O) a and (C n H 2n O The n) b is an integer of 2~4, a + b is 5-23. ]本発明の目的は、不織布の製造時に発煙が低減され、しかも、しかも初期親水性及び耐久親水性が共に優れるオレフィン重合体不織布に好適な繊維及び不織布を開発することである。本発明は、オレフィン系重合体100重量部に対して、下記化学式(1)で表されるポリ(オキシアルキレン)ジオールのジ脂肪酸エステルを0.5~5重量部及びポリ(オキシアルキレン)ソルビタン・トリ脂肪酸エステル(アルキレン基はエチレンまたはプロピレンまたはブチレン基であり、付加モル数は10~40、脂肪酸は炭素数が12~18のアルキル、又はアルキレン脂肪酸である。)を0.01~2.5重量部と含むオレフィン系重合体組成物からなる繊維を提供するものである。R1-COO-(CnH2nO)a-C6H12-O(CnH2nO)b-CO-R2・・・・式(1)[式中、R1及びR2は炭素数が11~17のアルキル基、であり、それぞれ同じであっても、異なってもよく、(CnH2nO)a及び(CnH2nO)bのnは2~4の整数であり、a+bは5~23である。]