ANTIADHESIVE MATERIAL
专利权人:
OTSUKA PHARMACEUT FACTORY INC;株式会社大塚製薬工場
发明人:
FUKUDA RITSU,福田 立,TAMURA HIROSHI,田村 浩史
申请号:
JP2018127855
公开号:
JP2018149414A
申请日:
2018.07.04
申请国别(地区):
JP
年份:
2018
代理人:
摘要:
PROBLEM TO BE SOLVED: To provide an antiadhesive material designed to change fluidity with time so as to exhibit gel shape high in fluidity at administration, and gel shape low in fluidity after administration to a dissected and stitched part.SOLUTION: A powdery antiadhesive material used by mixing with an aqueous solvent at use, containing alginic acid and/or a salt thereof, and designed to be used by mixing with the aqueous solvent so that viscosity at 37°C is 70 mPas s or less at the point of 5 minutes after mixing with the aqueous solution, and viscosity at 37°C is 120 mPas s or more at the point of 60 minutes after mixing, can achieve both of excellent operability and antiadhesive effect because it maintains a state having high fluidity at administration when mixing with the aqueous solvent at use at a clinical site and fluidity is reduced after administration to a dissected and stitched part.SELECTED DRAWING: None【課題】本発明の目的は、投与時には流動性が高いゲル状を示し、切開・縫合した部位に投与した後には流動性が低いゲル状を示すように、経時的に流動性が変化するように設計された癒着防止材を提供することである。【解決手段】使用時に水性溶媒と混合して使用される粉末状の癒着防止材であって、アルギン酸及び/又はその塩を含有し、且つ水性溶媒との混合後5分間の時点では37℃での粘度が70mPas・s以下であり、混合後60分間の時点では37℃での粘度が120mPas・s以上になるように水性溶媒と混合して使用されるように設定された癒着防止材は、臨床現場で使用時に水性溶媒と混合すると、投与する際には流動性が高い状態を保持し、切開・縫合した部位に投与した後には流動性が低くなり、優れた操作性と癒着防止効果を両立できる。【選択図】なし
来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充