PROBLEM TO BE SOLVED: To provide a construction method for an antibacterial concrete floor capable of achieving rationalization of construction by making only a necessary part exert antibacterial performance and excellent in durability.SOLUTION: Before placed concrete 1 is hardened, antibacterial agent slurry 2, in which fine-grained antibacterial agents 3, 3... are dispersed in predetermined quantities in water, is sprayed on a surface of the placed concrete 1. A surface layer part of the placed concrete 1 is impregnated with the antibacterial agents 3, 3... while the surface of the concrete 1, on which the antibacterial agent slurry 2 is sprayed, is leveled. Subsequently, an antibacterial concrete layer 5 containing the antibacterial agents 3, 3... is formed on the surface layer part of a concrete floor 5 by hardening of the placed concrete 1.COPYRIGHT: (C)2014,JPO&INPIT【課題】抗菌性能を必要な部分にのみ発揮させて施工の合理化を図れ、且つ、耐久性にも優れた抗菌性コンクリート床の構築方法の提供。【解決手段】打設したコンクリート1が硬化する前に、打設したコンクリート1の表面に所定量の細粒状の抗菌剤3,3...を水中に分散させてなる抗菌剤スラリー2を散布し、抗菌剤スラリー2が散布されたコンクリート1表面を均しつつ、打設したコンクリート1の表層部に抗菌剤3,3...を含浸させ、然る後、打設したコンクリート1の硬化によりコンクリート床5の表層部に抗菌剤3,3...を含有する抗菌性コンクリート層5が形成される。【選択図】図1