Homogeneous composition comprises 15-45 wt.% polyvinyl acetate, 10-30 wt.% vinyl laurate-vinyl acetate copolymers, 15-45 wt.% fillers, 5-30 wt.% waxes or fats, 1-10 wt.% plasticizers and 1-10 wt.% emulsifiers. Independent claims are also included for: (1) producing a homogeneous composition comprising mixing the polyvinyl acetate, vinyl acetate-vinyl laurate copolymer, filler, wax or fat, plasticizer and emulsifier in a discontinuous or continuous method at a temperature of 80-130[deg] C for a time period of 30-100 minutes; (2) a chewing gum comprising the composition, sugar or syrup, flavorings, optionally dyes, fruit acids, moisture-retention agents or polyols and sweeteners; and (3) producing a chewing gum, comprising mixing a homogeneous composition with polyols or sugar, syrup, flavorings, and optionally dyes, fruit acids, sweeteners and moisture-retention agents at approximately 60[deg] C.