A preparation method for a medical porous tantalum material, characterized in that: mixing tantalum powder and an aqueous solution of polyvinyl alcohol into a slurry, injecting the slurry into an organic foamed body by using pressuring by vibration, then drying, degreasing, sintering, cooling, and performing a heating process to produce the medical porous tantalum material, the mass concentration of the aqueous solution of polyvinyl alcohol being 2% to 8%, and the vibration frequency being 20 to 80 times/minute. The porous tantalum prepared using the present invention is applicable as a medical implant material for weight-bearing bone tissue replacement, and ensures both biocompatibility and mechanic properties.Procédé de préparation dun matériau de tantale poreux à usage médical caractérisé en ce que : une solution aqueuse dalcool polyvinlyique est liée à une suspension de poudre de tantale, la suspension est ajoutée moyennant pression vibratoire à un corps mousseux organique, le mélange étant, par la suite, soumis à séchage, décrassage, frittage, refroidissement et chauffage afin dobtenir un matériau de tantale poreux à usage médical, la concentration massique de la solution aqueuse dalcool polyvinylique étant de 2 à 8 % et la fréquence vibratoire de 20 à 80 fois/sec. Le tantale poreux ainsi obtenu satisfait aux exigences dutilisation dun matériau dimplant médical de substitution dun tissu osseux de support sans affecter ni sa biocompatibilité ni ses propriétés mécaniques.