摘要:
To provide a cellulose fine fiber whose dispersion has extremely high light transmittance and viscosity, and provide a method for producing the same.SOLUTION: Cellulose microfibers of this invention have a fiber width of 1 to 200 nm, a portion of the hydroxy groups of the cellulose fiber is substituted with a predetermined functional group, and an ester of phosphooxo acid is introduced, and the amount of the functional group introduced is more than 2.0 mmol per 1 g of cellulose fiber. Further, in producing this cellulose fine fiber, the cellulose fibers are added with the solution having a pH of less than 3.0, which contains an additive (A) containing at least one of phosphorus oxoacids and metal salts of phosphorus oxoacids and an additive (B) containing at least one of urea and an urea derivative, are heated, and fibrillated.SELECTED DRAWING: None【課題】セルロース微細繊維を分散液とした場合において、当該分散液の光透過度及び粘度が極めて高いものとなるセルロース微細繊維及びその製造方法を提供する。【解決手段】セルロース微細繊維は、繊維幅が1~200nmであり、セルロース繊維のヒドロキシ基の一部が所定の官能基で置換されてリンオキソ酸のエステルが導入されており、前記官能基の導入量がセルロース繊維1gあたり2.0mmol超とされている。また、このセルロース微細繊維を製造するにあたっては、セルロース繊維に、リンオキソ酸類及びリンオキソ酸金属塩類の少なくともいずれか一方を含む添加物(A)並びに尿素及び尿素誘導体の少なくともいずれか一方を含む添加物(B)からなるpH3.0未満の溶液を添加し、加熱し、解繊する。【選択図】なし
来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充