PROBLEM TO BE SOLVED: To provide a laminate capable of maintaining a removal effect of formaldehyde for a long time and to provide a method for producing the same.SOLUTION: There is provided a laminate 1 having a substrate 11, a drug-containing layer 12 and a coating layer 14, wherein the drug-containing layer 12 is disposed between the substrate 11 and the coating layer 14, the coating layer 14 is the uppermost surface layer of the laminate 1, the drug-containing layer 12 contains a microencapsulated formaldehyde reactant and a non-microencapsulated formaldehyde reactant, the coating layer 14 is obtained by blending one or both of a microencapsulated formaldehyde reactant and a non-microencapsulated formaldehyde reactant and is formed using a composition for forming a coating layer having a viscosity of 90 to 14200 mPa s.SELECTED DRAWING: Figure 1COPYRIGHT: (C)2019,JPO&INPIT【課題】ホルムアルデヒドの除去効果を長期間維持可能な積層体及びその製造方法の提供。【解決手段】基材11と、薬剤含有層12と、被覆層14と、を備えた積層体1であって、薬剤含有層12が、基材11と被覆層14と、の間に配置され、被覆層14が、積層体1の最表層であり、薬剤含有層12が、マイクロカプセル化されたホルムアルデヒド反応剤と、マイクロカプセル化されていないホルムアルデヒド反応剤と、を含有し、被覆層14が、マイクロカプセル化されたホルムアルデヒド反応剤と、マイクロカプセル化されていないホルムアルデヒド反応剤と、のいずれか一方又は両方が配合されてなり、かつ粘度が90~14200mPa・sである、被覆層形成用組成物を用いて形成されたものである、積層体1。【選択図】図1