摘要:
This invention provides a method for preparing a porous bone repair material, which comprises following steps of : proceeding a sulfonation reaction by reacting poly(aryl ether ketone) with a sulfuric acid solution to obtain a solution containing sulfonated poly(aryl ether ketone) adding said solution containing sulfonated poly(aryl ether ketone) to water to precipitate a solid sulfonated poly(aryl ether ketone) material containing liquid removing said liquid from said solid sulfonated poly(aryl ether ketone) material to obtain a porous bone repair material. Said method for preparing a porous bone repair material is easy to operate, and is easy to prepare a bone repair material.一種多孔性骨修復材的製備方法,包含以下步驟:將聚芳醚酮與硫酸溶液進行磺酸化反應,得到一含有磺酸化聚芳醚酮的溶液。將該含有磺酸化聚芳醚酮的溶液加入水中,以析出一含有液體的固態磺酸化聚芳醚酮材。去除該固態磺酸化聚芳醚酮材中的液體,以得到一多孔性骨修復材。該多孔性骨修復材的製備方法具有操作簡易的優點,並能製得多孔性的骨修復材。