PROBLEM TO BE SOLVED: To provide a method for manufacturing a bone-compatible titanium material by which a biologically active calcium-containing oxide layer can simply and inexpensively be formed on the surface of titanium or a titanium alloy.

SOLUTION: When manufacturing the bone-compatible titanium material, first a powder calcium hydroxide reagent 2 is mixed with distilled water 3 to create an alkaline processing agent (calcium hydroxide slurry) 4 in a slurry state including calcium. Then, a titanium or titanium alloy agent 5 is embedded into the slurry alkaline processing agent 4. Thermal processing (oxidation processing) is performed to the slurry alkaline processing agent 4 in a slurry state with a sample 5 embedded in the atmosphere. Thus, a calcium titanate layer is formed on the surface of the sample 5 and immediate below the calcium titanate layer, a titanium dioxide layer is formed.

COPYRIGHT: (C)2008,JPO&INPIT

来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充