Method for stretching a web of starting of a thermoplastic polymer material containing at least one polymer component of low melting point and at least one polymer component of high melting point, the method comprising the steps of: heating by at least one heating roller, the web of starting up a partially molten state, wherein the or polymeric components of low melting point are in the molten state and or the polymer components of high melting point not are in the molten state, and cooling driving the continuous sheet partially melted by a groove roller cooled, wherein the sheet is stretched between the at least one heating roller and groove roller cooled with a draw ratio of at least 1: 1.5.Procedimiento para el estiramiento de una lámina continua de partida de un material polímerico termoplástico, que contiene al menos un componente polímerico de bajo punto de fusión y al menos un componente polímerico de alto punto de fusión, comprendiendo el procedimiento las siguientes etapas: calentar, mediante al menos un rodillo de calentamiento, la lámina continua de partida hasta un estado parcialmente fundido, en el que el o los componentes polímericos de bajo punto de fusión se encuentran en el estado fundido y el o los componentes polímericos de alto punto de fusión no se encuentran en el estado fundido, y enfriar conduciendo la lámina continua parcialmente fundida por una ranura de rodillo enfriada, en el que la lámina es estirada entre el al menos un rodillo de calentamiento y la ranura de rodillo enfriada con una relación de estirado de al menos 1:1,5.