The method of obtaining polymer layers on the surface of titanium or titanium alloys on a polymer basis with medicinal products is characterised by the anode oxidation of titanium or titanium alloy in an aqueous bath containing calcium phosphorus of the concentration 0001 mol/dm3 -10 mol/dm3 using a compression voltage ranging from 0,1 V to 800 V, the anode current density of 5-500 A/dm2 and then the oxidised titanium or titanium alloy is placed in a polymer solution based on adipic acid derivatives,a dichloromethane-positive solvent and a medicinal product for the benefit of an antibiotic or an anti-inflammatory drug for the benefit of a non-steroidal or immunosuppressive agent or an antifungal or antiviral agent used in the treatment of hard circulating tissues, in quantities from 0000001 g/L to 1000 g/L, and then drying.Sposób otrzymywania warstw polimerowych na powierzchni tytanu lub stopów tytanu na bazie polimeru z lekami charakteryzuje się tym, że tytan lub stop tytanu utlenia się anodowo w kąpieli wodnej zawierającej podfosforyn wapnia o stężeniu 0,001 mol/dm3 - 10 mol/dm3 stosując napięcie zaciskowe w zakresie od 0,1 V do 800 V, anodową gęstością prądu w zakresie 5 - 500 A/dm2, a następnie tak utleniony tytan lub stop tytanu umieszcza się w roztworze polimeru na bazie pochodnej kwasu adypinowego, rozpuszczalnika korzystnie dichlorometanu i leku korzystnie antybiotyku lub leku przeciwzapalnego korzystnie niesteroidowy lub leku immunosupresyjnego lub leku przeciwgrzybicznego lub leku przeciwwirusowego stosowanego w leczeniu tkanek twardych okołowszczepowych, w ilości od 0,0001 g/L do 1000 g/L, a następnie suszy.