A process for preparing precipitated silica, is disclosed. The process includes preparing an aqueous solution of sodium silicate having a pH in a range of 10.6 to 10.8, simultaneously adding to said aqueous solution of sodium silicate, a sodium silicate solution, water and an acid in at least two phases to obtain a reaction mixture, wherein in an initial phase the sodium silicate solution, the water and the acid is added till the sodium ion concentration of the reaction mixture is in range of 0.13 normal to 0.57 normal and in a final phase the sodium silicate solution, the water and the acid is added till the sodium ion concentration of the reaction mixture is in a range of 0.3 to 0.9 normal; acidifying the reaction mixture with the acid to a pH in a range of 3 to 4.5, aging the reaction mixture to obtain precipitated silica and recovering the precipitated silica from the reaction mixture.L'invention concerne un procédé de préparation de silice précipitée. Le procédé comprend la préparation d'une solution aqueuse de silicate de sodium ayant un pH dans une plage de 10,6 à 10,8, l'ajout simultané à ladite solution aqueuse de silicate de sodium, d'une solution de silicate de sodium, d'eau et d'un acide dans au moins deux phases pour obtenir un mélange réactionnel, dans une phase initiale, la solution de silicate de sodium, l'eau et l'acide sont ajoutés jusqu'à ce que la concentration en ions sodium du mélange réactionnel soit dans une plage de 0,13 à 0,57 normale et dans une phase finale la solution de silicate de sodium, l'eau et l'acide sont ajoutés jusqu'à ce que la concentration en ions sodium du mélange réactionnel soit dans une plage de 0,3 à 0,9 normale; l'acidification du mélange réactionnel avec l'acide à un pH compris dans une plage de 3 à 4,5, le vieillissement du mélange réactionnel pour obtenir de la silice précipitée et la récupération de la silice précipitée à partir du mélange réactionnel.