TODD RYAN THOMPSON,ROBERT WAYNE GLENN JR.,UNGYEONG JUNG,CHANGWEI ZHU,CHUL B. PARK,RAYMOND KAR MAN CHU
申请号:
MX2015012308
公开号:
MX2015012308A
申请日:
2014.03.14
申请国别(地区):
MX
年份:
2016
代理人:
摘要:
Provided is a process for forming a dissolvable fiber, the process including (a) producing an extrudate from a twin screw extruder and (b) forming the extrudate into the dissolvable fiber. The dissolvable fiber includes (i) from about 10% to about 60% of one or more anionic surfactants (ii) from about 10% to about 50% of one or more water soluble polymers (iii) from about 1% to about 30% of one or more plasticizers and (iv) from about 0.01% to about 30% water. The one or more anionic surfactants have a Krafft point of less than about 30oC. The dissolvable fiber has an average diameter of from about 20 microns to about 1,000 microns.Se proporciona un proceso para formar una fibra soluble, el proceso comprende (a) producir un producto extrudido a partir de un extrusor de tornillo doble y (b) formar el producto extrudido en la fibra soluble. La fibra soluble incluye (i) de aproximadamente 10 % a aproximadamente 60 % de uno o más suríactantes aniónicos (ii) de aproximadamente 10 % a aproximadamente 50 % de uno o más polímeros solubles en agua (iii) de aproximadamente 1 % a aproximadamente 30 % de uno o más plastificantes y (iv) de aproximadamente 0.01 % a aproximadamente 30 % de agua. Uno o más suríactantes aniónicos tienen un punto Kraft menor que aproximadamente 30 °C. La fibra soluble tiene un diámetro promedio de aproximadamente 20 micras a aproximadamente 1000 micras.