PROBLEM TO BE SOLVED: To provide a method of producing apatite strontium carbonate which provides apatite strontium carbonate having good crystallinity with high purity and is simple and good in productivity and a method of producing a fine particle of apatite strontium carbonate suitable for coating applications.SOLUTION: A method of producing apatite strontium carbonate comprises mixing strontium hydrogenphosphate with 0.2 molar ratio of more, relative to strontium hydrogenphosphate, of a carbonate or 0.4 molar ratio or more of a hydrogencarbonate in water to react together. A method of a fine particle of apatite strontium carbonate comprises subjecting apatite strontium carbonate obtained by the method of producing apatite strontium carbonate to a wet dispersion treatment using a medium mill.COPYRIGHT: (C)2015,JPO&INPIT【課題】結晶性の良好な炭酸ストロンチウムアパタイトを高純度で得るための、簡便でかつ生産性の良好な炭酸ストロンチウムアパタイトの製造方法、およびコーティング用途に好適な炭酸ストロンチウムアパタイト微粒子の製造方法を与えること。【解決手段】水中に於いてリン酸水素ストロンチウムと、該リン酸水素ストロンチウムに対して0.2モル比以上の炭酸塩、または0.4モル比以上の炭酸水素塩を混合して反応を行う炭酸ストロンチウムアパタイトの製造方法。およびこれをメディアミルを使用して湿式分散処理を行う炭酸ストロンチウムアパタイト微粒子の製造方法。【選択図】なし