PROBLEM TO BE SOLVED: To provide a gel elastomer composition having proper hardness as well as capable of exhibiting excellent emollient effect without generating stickiness by easily releasing an oil agent even with light load and a gel sheet for cosmetics using the same.SOLUTION: A gel elastomer composition contains 100 pts.mass of (A) a styrenic thermoplastic elastomer mixture containing a low molecular weight styrenic thermoplastic elastomer (A1) and high molecular weight styrenic thermoplastic elastomer (A2) with a mass ratio of (A1)/(A2)=95/5 to 50/50, 500 to 4800 pts.mass of (B) an aliphatic hydrocarbon oil having kinetic viscosity at 37.8°C of 5 to 50 mm2/s and 60 to 1000 pts.mass of (C) aliphatic acid triglyceride having 8 to 22 carbon atoms, which is liquid at 20°C.SELECTED DRAWING: NoneCOPYRIGHT: (C)2017,JPO&INPIT【課題】本発明は、適度な硬さを有するとともに、軽い負荷でも油剤が容易に放出されることにより、べたつきを生じることなく優れたエモリエント効果を発揮することができるゲルエラストマー組成物、及びそれを用いた化粧用ゲルシートを提供することを目的とする。【解決手段】本発明のゲルエラストマー組成物は、低分子量のスチレン系熱可塑性エラストマー(A1)と、高分子量のスチレン系熱可塑性エラストマー(A2)とを、(A1)/(A2)=95/5~50/50の質量比で含む、スチレン系熱可塑性エラストマー混合物(A)100質量部に対し、37.8℃における動粘度が5~50mm2/sである脂肪族炭化水素油(B)500~4800質量部と、20℃で液体である炭素数8~22の脂肪酸トリグリセリド(C)60~1000質量部とを含有する。【選択図】なし