酸化鉄・オルガノポリシロキサンハイブリッド粉体及びその製造方法並びにそれを配合した化粧料
专利权人:
株式会社コーセー
发明人:
増渕 祐二,鈴木 一弘
申请号:
JP2010081548
公开号:
JP5584005B2
申请日:
2010.03.31
申请国别(地区):
JP
年份:
2014
代理人:
摘要:
PROBLEM TO BE SOLVED: To provide a process for producing a hybrid powder of an iron oxide and an organopolysiloxane which can inexpensively obtain a hybrid powder in a high yield.SOLUTION: The process for producing an iron oxide-organopolysiloxane hybrid powder comprises reacting iron (III) chloride (A) with an alkali to obtain iron (III) hydroxide (a) and adding an organopolysiloxane (B) represented by formula (1) (wherein Rs may be the same or different, each hydrogen or a 1-4C alkyl group X is a 2-4C alkylene group which may have an ether bond (-O-) and n is 1-12) to this iron (III) hydroxide (a) at a molar ratio of [(a):(B)] of 10:0.05 to 10:1.5 to allow the organopolysiloxane (B) to react with the iron (III) hydroxide (a).COPYRIGHT: (C)2012,JPO&INPIT【課題】安価かつ高収率にハイブリッド粉体が得られる酸化鉄とオルガノポリシロキサンのハイブリッド粉体の製造方法を提供する。【解決手段】(A)塩化鉄(III)をアルカリと反応させて(a)水酸化鉄(III)を得て、この(a)水酸化鉄(III)に(B)下記一般式(1)(式中、Rは同一または異なってもよく、水素原子または炭素数1~4のアルキル基を示し、Xはエーテル結合(-O-)を有していてもよい炭素数2~4のアルキレン基を示し、nは1~12である)で表されるオルガノポリシロキサンをモル比((a):(B))10:0.05~10:1.5で添加して反応させることを特徴とする酸化鉄・オルガノポリシロキサンハイブリッド粉体の製造方法。【選択図】図1
来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充