A method for preparing carbonate apatite from natural bones. The method includes obtaining cancellous bone particles treating the bone particles with hot water and an organic solvent repeating the treating step at least once drying the bone particles and heating the bone particles at 500° C. to 620° C. for 10 to 50 hours.