摘要:
SubjectIt is excellent in liquid permeability and is provided with a non-woven fabric excellent in dry feeling and taste obtained by suppressing liquid return.SolutionA laminated nonwoven fabric in which a thermally fused non-woven fabric layer (a) and a fine fiber nonwoven fabric layer (b) are laminated;As the fiber (FA) constituting the heat fusion nonwoven layer (a)At least the composite fiber (FA1) comprising at least the first thermoplastic resin composition (PA11) and the second thermoplastic resin composition (PA12) is usedFiber (FB) constituting said fine fiber nonwoven layer (b) isThe thermoplastic resin composition (PB) is used at leastAndA laminated non-woven fabric whose apparent specific volume (S1) of the thermal fusion nonwoven fabric layer (a) and the ratio (S1 / S2) of the apparent specific volume (S2) of the fine fiber nonwoven fabric (b) are 2.0 or more.No selection【課題】 通液性に優れているとともに、液戻りを抑制することで得られるドライ感や風合いに優れている不織布を提供することである。【解決手段】 熱融着性不織布層(A)と極細繊維不織布層(B)とが積層されてなる積層不織布であって、前記の熱融着性不織布層(A)を構成する繊維(Fa)として、少なくとも第1の熱可塑性樹脂組成物(Pa11)と第2の熱可塑性樹脂組成物(Pa12)とからなる複合繊維(Fa1)を少なくとも用いてなり、前記の極細繊維不織布層(B)を構成する繊維(Fb)が、熱可塑性樹脂組成物(Pb)を少なくとも用いてなり、さらに、前記熱融着性不織布層(A)の見かけの比容積(S1)と極細繊維不織布(B)の見かけの比容積(S2)の比(S1/S2)が2.0以上である積層不織布。【選択図】 なし
来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充