To provide a method for producing high-purity iron oxide nanoparticles by using nanoparticle producing cells.SOLUTION: A method includes the followings: a) a preliminary growth step including amplifying nanoparticle producing cells in preliminary growth medium and/or fed-batch medium; and b) a growth step including amplifying the nanoparticle producing cells generated from the preliminary growth step in the growth medium and/or the fed-batch medium, in which the preliminary growth medium and/or the growth medium and/or the fed-batch medium contains the followings per kilogram or per liter of the preliminary growth medium and/or the growth medium and/or the fed-batch medium: i) 0.005 gram or less of yeast extract and ii) 0.001 gram or less of CMR agent selected from boric acid and nitrilotriacetic acid, in which the fed-batch medium is medium supplementing preliminary growth and/or growth medium. Further, a larger number of nanoparticles is created in the growth step than the preliminary growth step.SELECTED DRAWING: None【課題】ナノ粒子産生細胞を使用して高純度酸化鉄ナノ粒子を産生する方法の提供。【解決手段】以下を含む方法:a)予備成長培地およびまたは流加培地でナノ粒子産生細胞を増幅することを含む予備成長ステップ、b)成長培地およびまたは流加培地での予備成長ステップから生じるナノ粒子産生細胞を増幅することを含む成長ステップ、ここで、予備成長培地およびまたは成長培地およびまたは流加培地は、予備成長培地およびまたは成長培地およびまたは流加培地のキログラムまたはリットルあたり以下を含む:i)0.005グラム以下の酵母エキス、およびii)0.001グラム以下のホウ酸およびニトリロ三酢酸から選択されるCMR剤、流加培地は、予備成長およびまたは成長培地を補う培地である。また成長ステップでは予備成長ステップより多くのナノ粒子が生成される。【選択図】なし