A composition is prepared to comprise (a) 50 to 99% by weight of an oily phase that is a liquid at 25°C, (b) 1 to 7% by weight of dextrin (palmitate/2-ethylhexanoate), and (c) 0.001 to 10% by weight of a coloring material and/or pearlescent agent other than a laminated film powder are contained, followed by making the viscosity thereof at 30°C when measured with a BL viscometer to be 3,000 to 20,000 mPa·s. In addition, (d) silicic acid anhydride and/or hydrophobized silicic acid anhydride is added thereto.