A method for manufacturing bioactive glass includes the steps below. A precursor and a polar solvent are mixed to form a mixed solution, in which the precursor includes a silicon precursor, a calcium precursor and a phosphorus precursor. The mixed solution is atomized to form a mixture droplet. The mixture droplet is oxidized in an environment of 500° C. to 900° C. to form the bioactive glass.