Wherein at least two kinds of fibers of the plurality of types of fibers each have a composition ratio of not less than 5.0% as a whole and a composition ratio of not less than 5.0% (Max), and the fiber having the smallest increase in surface area represented by the following formula (1) is used as the fiber (min), among the plural kinds of fibers having the surface area increase degree , The fiber (min) has a surface area increase rate of 3.0% or more lower than the fiber (max), the composition ratio of the fiber (max) to the entire mixed fibers is 30.0% (A) a surface area increase degree of not less than 1.20, (b) a porous material, and a pore specific surface area of not less than 5 m 2 / g. Surface area increase degree = (circumferential length in the fiber cross-section) / (circumferential length in the circle having the same cross-sectional area as the fiber cross-section) (1) It is possible to provide a fiber material made of fibers capable of efficiently adsorbing a substance to be removed in the liquid to be treated and a purification column in which such fibers are incorporated.횡단면 형상을 공통으로 하는 중실 섬유를 복수 종류 갖는 혼섬 섬유를 포함하고, 상기 복수 종류의 섬유 중 적어도 2종류는 상기 혼섬 섬유의 전체에 있어서의 구성 비율이 5.0% 이상이며, 상기 구성 비율이 5.0% 이상인 복수 종류의 섬유 중, 하기 식 (1)로 표현되는 표면적 증가도가 가장 높은 섬유를 섬유(max), 하기 식 (1)로 표시되는 표면적 증가도가 가장 낮은 섬유를 섬유(min)로 했을 때에, 섬유(min)는 섬유(max)에 비하여 표면적 증가도가 3.0% 이상 낮고, 섬유(max)의 상기 혼섬 섬유의 전체에 있어서의 구성 비율은 30.0% 이상, 섬유(min)의 상기 혼섬 섬유의 전체에 있어서의 구성 비율이 8.0% 이상이고, 또한, 섬유(max)는 (a) 표면적 증가도가 1.20 이상, (b) 다공질이고, 세공 비표면적이 5㎡/g 이상인 섬유 재료.표면적 증가도=(섬유 횡단면에 있어서의 둘레 길이)/(섬유 횡단면과 동일한 단면적을 갖는 원에 있어서의 원주 길이) (1)피처리액 중의 제거 대상 물질의 효율적인 흡착이 가능한 섬유를 사용하여 이루어지는 섬유 재료, 및 이러한 섬유가 내장된 정화 칼럼을 제공할 수 있다.