Methods of producing a dental product are disclosed. Certain methods include the steps of providing a pre-sintered blank made from a green body of ceramic material, performing a machining operation on the blank, and subsequently sintering the blank to its final density in a sintering operation performed at a temperature in the range of 1300° C. to 1650° C. The pre-sintered blank that is provided may have a strength in the range of 53-107 MPa.