PROBLEM TO BE SOLVED: To provide a superabsorbent polymer having improved odor prevention performance and a manufacturing method therefor.SOLUTION: There is provided a manufacturing method of an absorbent polymer, and/or a hydrogel polymer containing (α1) 20 to 99.999 wt.% of an unsaturated ethylene monomer or a salt thereof or an unsaturated ethylene monomer containing a protonated or quaternized nitrogen or a mixture thereof, (α2) 0 to 80 wt.% of an unsaturated monoethylene monomer copolymerizable with (α1), (α3) 0.001 to 5 wt.% of one or more kind of crosslinker, (α4) 0 to 30 wt.% of a water-soluble polymer, (α5) 0 to 20 wt.% or water, and (α6) 0 to 20 wt.% of one or more kind of additive (total weight of (α1) to (α6) is 100 wt.%) and treated by a peroxo compound of 0.0001 to 3 wt.% based on acrylic acid after polymerization.COPYRIGHT: (C)2015,JPO&INPIT【課題】改善された臭気抑制性能を有する超吸収性ポリマー及びその製造方法の提供【解決手段】(α1)20~99.999重量%のエチレン性不飽和酸基含有モノマー又はその塩、又はプロトン化又は四級化窒素を含有するエチレン性不飽和モノマー、又はそれらの混合物と、(α2)0~80重量%の(α1)と共重合可能なモノエチレン性不飽和モノマーと、(α3)0.001~5重量%の1種以上の架橋剤と、(α4)0~30重量%の水溶性ポリマーと、(α5)0~20重量%の水と、(α6)0~20重量%の1種以上の添加剤とからなり((α1)~(α6)の合計重量は100重量%)、重合後に、アクリル酸に対して、0.0001~3重量%のペルオキソ化合物で処理した吸水性ポリマー、ヒドロゲルポリマーの製造方法。【選択図】なし