摘要:
A method of producing a solid solution in the form of granules or a powder form of the low solubility agent, take a molecular dispersed form in the auxiliary matrix, low soluble substance is a solution containing the matrix auxiliaries and low solubility active ingredient A method of producing by spraying, a step of dissolving a poorly soluble materials and steps, is heated to a temperature above its boiling point at atmospheric pressure an aqueous suspension of the low solubility agent in the presence of the matrix auxiliaries is 90 ℃ ~350 ℃ temperature of the spray solution before comprises the step of solidified by spray drying a solution containing the matrix auxiliaries and low soluble substance is then introduced to the spray device, the above method. [Selection] Figure Figure 1低溶解性物質の粉体形態または顆粒形態の固溶体を生成する方法であって、低溶解性物質は助剤マトリックス中で分子分散形態をとり、低溶解性活性成分とマトリックス助剤を含む溶液を噴霧することにより生成する方法であり、マトリックス助剤の存在下で低溶解性物質の水性懸濁液を常圧でのその沸点より高い温度に加熱するステップ、および低溶解性物質を溶解するステップ、続いて低溶解性物質とマトリックス助剤を含む溶液を噴霧乾燥することによって固体化するステップを含み、噴霧装置に導入する前のスプレー溶液の温度が90℃~350℃である、上記方法。【選択図】 図1
来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充