BOHEN, John Michael,ANDERSON-GABER, Amy Christine,GRAHN, Anita Marie
申请号:
ES13746639
公开号:
ES2646199T3
申请日:
2013.02.05
申请国别(地区):
ES
年份:
2017
代理人:
摘要:
A method for forming a complex of large particles having a particle size of 100 micrometers to 200 micrometers, said method comprising the steps of: a) combining a hydrolyzed corn starch polymer, a starch / cellulose polymer, a hydrogenated phospholipid , and gum arabic in a cosmetically acceptable carrier to form a premix composition. b) heating said premix at 85 ° C for 15 minutes; and c) cooling said composition to room temperature, wherein said composition comprises from 0.01% to 10% by weight of hydrolyzed corn starch polymer, from 0.01% to 10% by weight of starch / cellulose polymer, of 0.1 to 2% by weight of hydrogenated phospholipid and 0.01 to 3% by weight of gum arabic, based on the total weight of the composition, and wherein said composition is not homogenized.Un método para formar un complejo de partículas grandes que tienen un tamaño de partícula de 100 micrómetros a 200 micrómetros, dicho método comprendiendo los pasos de: a) combinar un polímero de almidón de maíz hidrolizado, un polímero de almidón/celulosa, un fosfolípido hidrogenado, y goma arábiga en un portador cosméticamente aceptable para formar una composición de premezcla. b) calentar dicha premezcla a 85º C durante 15 minutos; y c) enfriar dicha composición a temperatura ambiente, en donde dicha composición comprende del 0,01% al 10% por peso de polímero de almidón de maíz hidrolizado, del 0,01% al 10% por peso del polímero de almidón/celulosa, del 0,1 al 2% por peso de fosfolípido hidrogenado y del 0,01 al 3% por peso de goma arábiga, en base al peso total de la composición, y en donde dicha composición no está homogeneizada.