摘要:
PROBLEM TO BE SOLVED: To provide a colloidal solution of platinum, which does not contain a protective agent, hardly causes coagulation or precipitation even if the concentration is high, and shows superior long-period stability.SOLUTION: The colloidal solution of platinum comprises a platinum colloid comprising platinum particles and a solvent of water or a mixture solvent including water and an organic solvent, and does not contain the protective agent, wherein the platinum content in the colloidal solution of platinum is 300 to 20,000 ppm, the pH is 5.0 to 12.0 and the electrical conductivity is 100 mS/m or less. The colloidal solution of platinum can be produced by reducing platinum ions in a platinum salt solution to form the platinum particles, but the production process needs to include the steps of: adjusting the pH of and the concentration of dissolved oxygen in the platinum salt solution before the reduction step and ultrafiltrating the colloidal solution of platinum obtained after the reduction step to adjust the electrical conductivity and the pH.COPYRIGHT: (C)2010,JPO&INPIT【解決課題】保護剤を含まない白金コロイド溶液に関し、高濃度であっても、凝集や沈殿を生じにくく、長期間安定性に優れるものを提供する。【解決手段】本発明は、白金粒子からなる白金コロイドと、水又は水及び有機溶媒の混合溶媒よりなる溶媒とからなる保護剤を含まない白金コロイド溶液において、白金コロイド溶液中の白金含有量が300~20000ppm、かつ、溶液はpH5.0~12.0、電気伝導度100mS/m以下である白金コロイド溶液である。本発明に係る白金コロイド溶液は、白金塩溶液中の白金イオンを還元して白金粒子を形成することにより製造可能であるが、還元工程前に白金塩溶液のpH、溶存酸素濃度を調整する工程、及び、還元工程後に得られた白金コロイド溶液を限外ろ過して電気伝導度を調整すると共にpHを調整する工程、を有することが必要である。【選択図】なし
来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充