인공 관절 및 그 제조 방법
专利权人:
LEE; CHAE WON
发明人:
LEE, CHAE WON,이채원
申请号:
KR1020110019268
公开号:
KR1020120100404A
申请日:
2011.03.04
申请国别(地区):
KR
年份:
2012
代理人:
摘要:
PURPOSE: An artificial joint and a manufacturing method thereof are provided to improve bio-compatibility and anti-wearing property.CONSTITUTION: A manufacturing method of an artificial joint is comprised as follows. An artificial joint structure(100) is formed by processing titanium. Air is exhausted to make the vacuum of the inside of a chamber at 1x10^-5 torr by operating vacuum equipment connected to the chamber. A coating layer(300) is formed in the thickness of 0.5-10 micrometers. The artificial joint comprises a joint structure, an intermediate layer(200), and a coating layer. The intermediate layer is formed on the surface of the joint structure. The coating layer is spread on the intermediate layer. The thickness of the intermediate layer is 0.1-0.5 micrometers.COPYRIGHT KIPO 2013본 발명은 티타늄 구조체에 생체 적합성과 내마모성이 우수한 질화 티타늄 물질을 피복한 인공 관절 및 그 제조하는 방법에 관한 것이다. 본 발명에 의한 인공 관절은, 관절 구조체 상기 관절 구조체의 표면에 형성되고, 티타늄 및 지르코늄 중 적어도 어느 하나를 포함하는 중간층 그리고 상기 중간층 위에 도포되고, 질화 티타늄 및 질화 지르코늄 중 적어도 어느 하나를 포함하는 피복층을 포함한다. 또한, 본 발명에 의한 인공 관절 제조 방법은, 관절 구조체를 형성하는 단계 증착 챔버 내에 티타늄 및 지르코늄 중 적어도 어느 하나를 포함하는 타겟 물질과 상기 관절 구조체를 장착하는 단계 상기 타겟 물질을 증착하여 상기 관절 구조체의 표면에 티타늄 및 지르코늄 중 적어도 어느 하나를 포함하는 중간층을 형성하는 단계 그리고 상기 챔버 내에 반응 가스를 투입하면서 상기 타겟 물질을 증착하여, 상기 관절 구조체의 표면에 상기 반응 가스와 상기 타겟 물질의 화합물을 포함하는 피복층을 형성하는 단계를 포함한다. 본 발명은 자연 관절과 거의 동일한 착용감으로 인해 거부감이 없고 반영구적으로 사용할 수 있는 인공 관절을 제공한다.
来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充