焼結体の製造方法
专利权人:
株式会社IHI
发明人:
寒川 喜光,鬼頭 浩,飴山 恵,野方 誠
申请号:
JP2007014493
公开号:
JP4952912B2
申请日:
2007.01.25
申请国别(地区):
JP
年份:
2012
代理人:
摘要:

PROBLEM TO BE SOLVED: To provide a method for producing a component having a thin part with a thickness of &le1 mm, having low surface roughness and having high sintered density and sintering strength without performing secondary working.

SOLUTION: The method includes: a stage where a molding material comprising metal powder and an organic binder is subjected to injection molding, so as to obtain a molded body and a degreasing-sintering stage where the molded body is degreased and sintered, so as to obtain a sintered compact. The above metal powder has the average grain size of 1 to 6 &mum, and is selected from stainless steel alloy powder, titanium alloy powder and/or alloy precursor powder forming a stainless steel alloy or a titanium alloy by sintering, and the ratio of the organic binder in the molding material is 40 to 50 vol.% of the whole quantity of the molding material. In the degreasing-sintering stage, the sintering maximum temperature is 900 to 1,200°C, the temperature rising rate in the temperature zone of 100 to 400°C is &le100°C/hr, and the temperature rising rate in the temperature zone of 600 to 800°C is &le200°C/hr.

COPYRIGHT: (C)2008,JPO&INPIT

来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充