摘要:
[Problem] To provide: a resin composition for cutting such that cutting time is reduced and an object which is to be cut and has an excellent external appearance can be produced therefrom; a resin molded body for cutting that includes the resin composition for cutting; and a method for manufacturing the same. [Solution] The resin composition for cutting comprises, as a basic composition, a total of 100 weight% including 40 to 97 weight% of a resin and 60 to 3 weight% of an inorganic filler, and has a cuttability parameter of 100 or less, which is calculated from the heat deflection temperature and the tensile modulus.L'invention fournit une composition de résine pour découpe excellente en termes de raccourcissement de durée de découpe et d'apparence d'objet à découper, un article moulé en résine pour découpe contenant cette composition de résine pour découpe, et un procédé de fabrication de celui-ci. La composition de résine pour découpe de l'invention a pour structure de base 100% en masse au total de 40 à 97% en masse d'une résine et de 60 à 3% en masse d'un matériau de charge inorganique. Ses paramètres de découpe calculés à partir de sa température de déformation à la chaleur et de son module d'élasticité à la traction sont inférieurs ou égaux à 100.【課題】切削時間の短縮及び被切削物の外観が優れた切削用樹脂組成物、この切削用樹脂組成物を含む切削用樹脂成形体、及びその製造方法を提供する。 【解決手段】 切削用樹脂組成物は、40~97重量%の樹脂と60~3重量%の無機充填材とを有する合計100重量%を基本組成とする樹脂組成物であって、熱変形温度及び引張弾性率から算出される切削性パラメータが100以下である。
来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充