Problem to be solved: to provide a stretched porous laminated film which has excellent tactile feeling and flexibility and suppresses the occurrence of unpleasant sound generated when the film is rubbed and has a tensile strength and a heat resistance to enable stable film conveyance.Solution: polyolefin resin (y) having a density of 0.910 g / cm3 or more is 25 mass% to 54% by massA (I) layer comprising a resin composition (y) comprising an inorganic filler (a) of 46 to 75% by weightA polyolefin resin (z) having a density of less than 0.850 g / cm3 or greater than 0.910 g / cm3 was 25% to 54% by massHaving an inorganic filler (a) having at least two layers of a (II) layer comprising a resin composition (z) comprising 46 to 75% by weightThickness ratio of the (II) layer to total thicknessIf the layer (2) is two or more layers, the thickness ratio of the total thickness is set.A stretched porous laminated film characterized by 35% or more of 99% or less.No selection【課題】 柔軟性と風合いといった優れた触感を有するとともに、フィルムの擦れ時に生じる不快な音の発生を抑制し、かつ、フィルムの安定的な搬送を可能にするための引張強度を有し、かつ、耐熱性を兼ね備えた延伸多孔積層フィルムの提供。【解決手段】 密度が0.910g/cm3以上のポリオレフィン系樹脂(y)を25質量%~54質量%、無機充填材(A)を46質量%~75質量%含む樹脂組成物(Y)からなる(I)層と、密度が0.850g/cm3以上0.910g/cm3未満のポリオレフィン系樹脂(z)を25質量%~54質量%、無機充填材(A)を46質量%~75質量%含む樹脂組成物(Z)からなる(II)層の少なくとも2層を有し、全厚さに対する前記(II)層の厚さ比率(ただし、(II)層を2層以上有する場合はその合計厚さの厚さ比率とする。)が35%以上99%以下であることを特徴とする延伸多孔積層フィルム。【選択図】 なし
来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充