Method of manufacturing a composite block intended for the manufacture of a dental prosthesis, said procedure comprising the following steps: a) infiltrating a support of a porous ceramic material by means of a liquid resin; b) harden the resin in a liquid state that permeates the support; characterized in that, in step b), the resin in a liquid state is subjected to a pressure greater than 300 bar, and by which a volume of resin in a liquid state of greater than at least 2% is penetrated and hardened to the volume of the open pores of the support, said volumes being measured at a temperature of 20 ° C and under a pressure of 1 bar.Procedimiento de fabricación de un bloque de material compuesto destinado a la fabricación de una prótesis dental, comprendiendo dicho procedimiento las etapas siguientes: a) infiltrar un soporte de un material cerámico poroso mediante una resina en estado líquido; b) endurecer la resina en estado líquido que impregna el soporte; caracterizado por que, en la etapa b), la resina en estado líquido se somete a una presión superior a 300 bares, y por que se hace penetrar y endurecer en el soporte un volumen de resina en estado líquido superior en al menos un 2% al volumen de los poros abiertos del soporte, midiéndose dichos volúmenes a una temperatura de 20ºC y bajo una presión de 1 bar.