PROBLEM TO BE SOLVED: To provide hydrogel compositions prepared from an amine component and a glycidyl ether component, and suitable for being used in situ, because of its biocompatibility and partially its excellent stability.SOLUTION: The present invention is for an in situ formed hydrogel polymer composition, comprising: (a) a first amount of a diamine; and (b) a second amount of a polyglycidyl ether; in which each of (a) and (b) are present in a mammal or in a medical device located in a mammal in an amount to produce an in situ formed hydrogel polymer that is biocompatible and has a cure time after mixing of from about 10 seconds to about 30 minutes. The volume of the hydrogel polymer swells less than 30 percent after curing and hydration.【課題】生体適合性であり、また部分的にはその優れた安定性により、インビボで使用するのに適した、アミン成分とグリシジルエーテル成分とから調製されるヒドロゲル組成物を提供する。【解決手段】(a)第1の量のジアミンと(b)第2の量のポリグリシジルエーテルとを含むその場で形成されるヒドロゲルポリマー組成物であって、(a)及び(b)の各々が、生体適合性であるその場で形成されるヒドロゲルポリマーを生成する量で哺乳動物内又は哺乳動物内に置かれた医療装置中に存在し、かつ約10秒から約30分の混合後の硬化時間を持っており、該ヒドロゲルポリマーの容積が、硬化及び水和後に30%未満で膨潤することを特徴とする組成物。【選択図】なし
来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充