Described herein is an absorbent article including (a) an absorbent core, a first nonwoven material, a second nonwoven material, and a bond area; and (b) a polymeric filler composition disposed within the bond area. The polymeric filler composition has less than 1% of a tackifier. The polymeric filler composition is chosen from a propylene butene copolymer, a polypropylene homopolymer, a propylene ethylene copolymer, and mixtures thereof. The polymeric filler composition has a Tensile Strength at Yield of from about 0.5 MPa to about 10 MPa. The bond area has a Peak Peel Strength of from about 0.1 N/cm to about 9 N/cm after exposure to a skin-protecting material for 24 hours.