The present invention relates to a method of fabricating an improved lithium silicate glass ceramic and to that material for the manufacture of blocks for dental appliances using a CAD/CAM process and hot pressing system. The lithium silicate material has a chemical composition that is different from those reported in the prior art with 1 to 10% of germanium dioxide in final composition. The softening points are close to the crystallization final temperature of 800° C. indicating that the samples will support the temperature process without shape deformation.