To provide a mixture having reverse wavelength dispersion property or low wavelength dispersion property, hardly generating deposition when applied to a substrate and dried, a polymerizable composition hardly being released from a substrate and hardly generating crack when a film-like polymerization obtained by polymerizing a polymerizable composition containing the mixture is bent, and further a polymer obtained by polymerizing a polymerizable liquid crystal composition containing the material and an optical anisotropic material using the polymer.SOLUTION: There are provided a mixture comprising a compound represented by a general formula (I-AA), a compound represented by a general formula (I-AI), and a compound represented by a general formula (I-IA), with percentages of the compound represented by the general formula (I-AA), the compound represented by the general formula (I-AI), and the compound represented by the general formula (I-IA) are 20 mass% to 80 mass%, 10 mass% to 40 mass%, and 10 mass% to 40 mass% respectively, a polymerizable composition, a polymerizable liquid crystal composition containing the mixture, a polymer obtained by polymerizing the polymerizable liquid crystal composition, and an optical anisotropic material using the polymer.SELECTED DRAWING: None【課題】 本発明が解決しようとする課題は、基材に塗布し乾燥させた際に析出が起こりにくい逆波長分散性又は低波長分散性を有する混合物を提供し、当該混合物を含有する重合性組成物を重合して得られるフィルム状の重合物を折り曲げた場合に、基材から剥離しにくく、割れが生じにくい重合性組成物を提供することである。さらに、当該材料を含む重合性液晶組成物を重合させることで得られる重合体及び当該重合体を用いた光学異方体を提供することである。【解決手段】 本願発明は一般式(I-AA)で表される化合物、一般式(I-AI)で表される化合物及び一般式(I-IA)で表される化合物からなる混合物であり、当該混合物中における一般式(I-AA)で表される化合物、一般式(I-AI)で表される化合物及び一般式(I-IA)で表される化合物の比率が各々20質量%から80質量%、10質量%から40質量%及び10質量%から40質量%である混合物を提供し、併せて当該混合物を含有する重合性組成物、重合性液晶組成物、当該重合性液晶組成物を重合させることにより得られる重合体及び当該重合体を用いた光学異方体を提供する。【選択図】 なし