VINYL FIXING SPRING FOR A GREEN HOUSE AND A MANUFACTURING METHOD THEREOF INCLUDING QUENCHING THROUGH HEAT TREATMENT
专利权人:
KIM; JONG HAN
发明人:
KIM, JONG HAN,김종한
申请号:
KR1020100076072
公开号:
KR1020120013822A
申请日:
2010.08.06
申请国别(地区):
KR
年份:
2012
代理人:
摘要:
PURPOSE: A vinyl fixing spring for a green house and a manufacturing method thereof are provided to improve the durability of a spring by forming coating on the surface of spring steel.CONSTITUTION: A method for manufacturing a vinyl fixing spring for a green house comprises the steps of: arranging semi-products, which are heated and air-cooled, separately from adjacent ones in a tray and heating the semi-products using an electric furnace to 250~270°C, immersing a coating liquid, which is composed of distilled water 33 weight%, an emulsifier 33 weight%, cation class paint 33 weight%, and solvent 1 weight%, for 1~3 seconds to form a coating layer(10c) of 15~20&mu, and drying a spring(10) with the coating layer in a drying furnace maintaining a temperature of 170~200°C.COPYRIGHT KIPO 2012본 발명은 비닐하우스의 비닐고정용 스프링 및 그 제조방법에 관한 것으로서, 스프링 표면의 부식을 방지하고, 강성을 높여서 고정력을 향상시킬 수 있게 하며, 또한 생산성 향상과 제조원가 절감을 기대할 수 있는 비닐하우스의 비닐고정용 스프링 및 그 제조방법을 제공코자 하는 것이다.즉, 본 발명은 신선(新選)작업된 아연도금된 고장력 스프링강을 고정부와 연결부가 연속적으로 형성되도록 지그재그식으로 절곡하고, 250~300℃ 온도로 3~6시간 가열 후 공랭하는 공정으로 비닐하우스의 비닐고정용 스프링을 제조함에 있어서상기 가열 후 공랭한 반제품을 이웃하는 것들과 분리되도록 트레이에 정렬한 상태에서 전기로를 이용하여 250~270℃의 온도가 되도록 가열하는 외장전처리공정과 중량비로 증류수33%와, 유화제33%와, 카치온계 도료33%와 용제1%를 혼합 조성한 피막도료액에 1~3초 동안 침지하여 도막 두께는 15~20μ이 되도록 피막도장층을 형성하는 외장피막공정과 외장피막공정을 통해서 피막도장층이 형성된 스프링을 170~200℃ 온도를 유지하는 건조로에서 20~30분 건조하는 건조공정의 제조방법과 그 제조방법으로 제조한 비닐하우스의 비닐고정용 스프링을 제공한 것이다.
来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充