ÉLÉMENT D'ALIMENTATION EN FER POUR EAU ENVIRONNEMENTALE, PROCÉDÉ DE MAINTENANCE DE L'ÉLÉMENT D'ALIMENTATION EN FER ET PROCÉDÉ D'ALIMENTATION DE FER À UNE EAU ENVIRONNEMENTALE
专利权人:
石井商事株式会社;NATIONAL INSTITUTE OF TECHNOLOGY;ISHII CORPORATION;独立行政法人国立高等専門学校機構
发明人:
KOJIMA, Akira,小島 昭,FUJISHIGE, Masao,藤重 昌生,ISHII, Toshiaki,石井 敏明,小島 昭,藤重 昌生,石井 敏明
申请号:
JPJP2015/004054
公开号:
WO2016/024408A1
申请日:
2015.08.14
申请国别(地区):
JP
年份:
2016
代理人:
摘要:
The present invention comprises an iron member, a carbon member and a conduction member, wherein the iron member and the carbon member are arranged without constraining each other; the conduction member has a volume resistivity of 10-4 Ω·m or less; and the conduction member connects the iron member and the carbon member and continually keeps the carbon member and the iron member in a good state of contact, thereby allowing iron to be efficiently supplied to environmental water.La présente invention comprend un élément en fer, un élément en carbone et un élément de conduction, l'élément en fer et l'élément en carbone étant disposés sans contrainte mutuelle ; l'élément de conduction a une résistivité volumique de 10-4 Ω·m ou moins ; et l'élément de conduction relie l'élément en fer et l'élément en carbone et maintient en continu l'élément en carbone et l'élément en fer dans un bon état de contact, ce qui permet au fer d'être alimenté de manière efficace à une eau environnementale.本発明に従い、鉄材と炭素材と導通材とからなり、該鉄材と該炭素材とは相互に拘束すること無く配置され、該導通材の体積抵抗率を10-4Ω・m以下とし、該導通材が該鉄材と該炭素材とを接続し、炭素材と鉄材との接触状態を常に良好に保つことで効率よく環境水へ鉄分を供給することができる。
来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充