Disclosed are: a biodegradable coating composition for a mulching paper; and a mulching paper. Out of these, the biodegradable coating composition for a mulching paper comprises: 45-72 parts by weight of spring water, the spring water being made by immersing a mineral material powder, which has a particle size distribution of 400-700 mesh and includes a sericite powder, in water contained in a container for 10-20 days to thereby allow mineral components of the mineral material to dissolve in water; 3-8 parts by weight of a charcoal powder having a particle size of 1,000-3,000 mesh; 8-13 parts by weight of a calcium liquid; 5-15 parts by weight of a filler containing a sulfur powder, an illite powder, and an expanded vermiculite powder; 5-8 parts by weight of starch; and 10-20 parts by weight of an additive. [Representative drawing] figure 1L'invention concerne : une composition de couchage biodégradable pour un papier de paillage ; et un papier de paillage. Parmi ceux-ci, la composition de couchage biodégradable pour un papier de paillage comprend : 45 à 72 parties en poids d'eau de source, l'eau de source étant obtenue par immersion d'une poudre de matière minérale, qui a une distribution de la taille des particules de 400 à 700 mesh et qui comprend une poudre de séricite, dans de l'eau contenue dans un récipient pendant 10 à 20 jours pour permettre ainsi aux composants minéraux de la matière minérale de se dissoudre dans l'eau ; 3 à 8 parties en poids d'une poudre de charbon de bois ayant une taille des particules de 1 000 à 3 000 mesh ; 8 à 13 parties en poids d'un liquide calcique ; 5 à 15 parties en poids d'une charge contenant une poudre de soufre, une poudre d'illite et une poudre de vermiculite expansée ; 5 à 8 parties en poids d'amidon ; et 10 à 20 parties en poids d'un additif. [Dessin représentatif] Figure 1멀칭지용 생분해성 코팅조성물 및 멀칭지가 개시되어 있다. 이 중, 멀칭지용 생분해성 코팅조성물은 물이 수용된 용기에 견운모 분말이 포함된 400~700 메쉬의 입도 분포를 갖는 광물질 분말을 10~20일 침지시킴에 따라, 광물질의 미네랄 성분이 물에 녹아 들어가게 하여